4 Open time : 12-15 minutes
5 Pressing time for handling strength:
(a) HPL to particle board/MDF/Plywood 6-8 hrs @ 25degree centigrade RH 65% OR 4 min @ 90 degree centigrade & 80 bar pressure
  (b) Wood to wood 6-8 hrs @ 25 degree centigrade RH 65%
6 Coverage : 3.5sq mt/kg

Application Instructions

1. Surfaces to be bonded should be free from oil/grease/dust & excess moisture.
2. Surfaces to be bonded should be properly leveled.
3. Stir contents before use.
4. Apply even coats on both the surfaces.
 
  next >> 1 2 3 4